• img

factory low price Plastic Film For Thermoforming - MESIM BOPA With Balanced Physical Properties And Converting – Changshu


Product Details

Related Video

Feedback (2)

Our primary purpose is to give our shoppers a serious and responsible company relationship, giving personalized attention to all of them for stretch nylon film , laminating film material , thermal lamination pouch film , Your aid is our everlasting power! Warmly welcome clients in your own home and abroad to go to our enterprise.
factory low price Plastic Film For Thermoforming - MESIM BOPA With Balanced Physical Properties And Converting – Changshu Detail:

Features Benefits
● Good oxygen/aroma barrier
● Outstanding isotropy performance in printing and retort
● Longer shelf life and better freshness
● Excellent converting performance and registration accuracy
● Excellent tensile strength, anti-punch and anti-impact properties
● High flex-crack resistance
● Wide temperature range in application
● Excellent transparency and gloss
● Capacity with excellent packaging safety to apply to heavy packaging, sharp and rigid products.
● Minimum distortion after retort

SHA can be used for producing the high-grade packaging within12 colors, sealing width ≤10cm and needs printing registration. It is not easy to warp and curl after 125℃ retorting. It’s recommended to be used for non-heavy packaging products with single bag capacity less than 2kg, for example, retort pouch and cup lid with delicate patterns.

Thickness /μm Width/mm Treatment Retortability Printability
15 300-2100 single/both side corona ≤121℃ ≤12 colors

Notice: retortability and printability are depending on customers’ lamination and printing processing condition.

Performance BOPP BOPET BOPA
Puncture Resistance
Flex-crack Resistance ×
Impact Resistance
Gases Barrier ×
Humidity Barrier ×
High Temperature Resistance
Low Temperature Resistance ×

bad×      normal△      quite good○      excellent◎

1
2
2121

The Small Dot/Shallow Net Lost

Print dots are missing or missed in the shallow position of the printed pattern (generally less than 30% of the dot, serious in 50% of the dot will also appear).

Causes:

Ink fineness is not enough, resulting in some large particles of ink cannot be filled to the network of shallow holes;

● Ink concentration is too thick, resulting in poor printing, the formation of dot hollowing;

● Scraper pressure is too large resulting in small amount of ink, ink supply is uneven, resulting in the loss of small dots;

● The use of too much quick-drying solvent, resulting in the ink drying up in the net hole and unable to attach to the film during the transfer process of the shallow net part;

● Printing speed is too slow, in the ink drying up in the net hole during the transfer process;

● Film surface is too rough; the underlying ink is not smooth.

Related Suggestions:

✔ Choose fineness ≤15μm ink;

✔ Appropriate dilute ink viscosity;

✔ The doctor blade should be adjusted to just scrape the ink, not to put too much pressure;

✔ Use less quick-drying solvent to adjust the drying speed of ink on the plate roller;

✔ Try to ensure that the speed of more than 160m/min printing.


Product detail pictures:

factory low price Plastic Film For Thermoforming -
 MESIM BOPA With Balanced Physical Properties And Converting  – Changshu detail pictures


Related Product Guide:

That has a positive and progressive attitude to customer's interest, our organization consistently improves our products quality to satisfy the demands of shoppers and further focuses on safety, reliability, environmental specifications, and innovation of factory low price Plastic Film For Thermoforming - MESIM BOPA With Balanced Physical Properties And Converting – Changshu , The product will supply to all over the world, such as: Marseille , Serbia , Guyana , We welcome you to visit our company & factory and our showroom displays various products and solutions that will meet your expectations. Meanwhile, it is convenient to visit our website. Our sales staff will try their best to supply you with the best services. If you will need more information, please do not hesitate to contact us via E-mail, fax or telephone.
  • The sales manager is very patient, we communicated about three days before we decided to cooperate, finally, we are very satisfied with this cooperation!
    5 Stars By Gwendolyn from Bangalore - 2017.10.25 15:53
    The factory workers have rich industry knowledge and operational experience, we learned a lot in working with them,we are extremely grateful that we can encount a good company has excellent wokers.
    5 Stars By Heloise from Malta - 2018.03.03 13:09
    Write your message here and send it to us